Skip to Content

Flange Material Grades: How to Choose

James Blue, Piping Materials Specialist

Flange Material Grades: How to Choose

Choose the flange material from the design temperature, the design pressure and the media. Price is the last screen. Carbon steel, low-temperature carbon steel, chrome-moly alloy, stainless and duplex each exist because one of those three limits rules out the cheaper grade.

The Grades and the Limit Each One Answers

The table is a selection screen. It is not a temperature rating. The allowable pressure at a given temperature comes from the pressure-temperature tables for that material group in the flange standard. A grade listed here can still be the wrong choice once those tables are checked.

GradeSpecificationThe limit it is meant to answer
Carbon steelASTM A105Ordinary temperature and non-corrosive media
Low-temperature carbon steelASTM A350 LF2Impact-tested service below the A105 range
Low-temperature carbon steelASTM A350 LF3Colder service than LF2, still impact tested
1-1/4Cr-1/2MoASTM A182 F11Elevated temperature above carbon steel
2-1/4Cr-1MoASTM A182 F22Higher temperature, including hydrogen service
9Cr-1Mo-VASTM A182 F91Creep, where F22 is no longer enough
304 stainlessASTM A182 F304Corrosion that carbon steel cannot take
316 stainlessASTM A182 F316Chlorides that pit 304
Duplex 2205ASTM A182 F51Chloride stress corrosion, with higher strength
Super duplex 2507ASTM A182 F53More aggressive chloride service than 2205

Start with Temperature

If the design temperature is low enough that carbon steel loses toughness, move to an impact-tested grade. The ASTM A350 LF2 low-temperature carbon steel flange is the common step. LF3 is the step below that. The test temperature and the required energy come from the material specification and the design code, so quote those rather than a rule of thumb.

If the design temperature is high enough that carbon steel loses allowable stress, move to a chrome-moly or stainless grade and read the pressure-temperature table. Do not keep A105 and "add a corrosion allowance" to solve a temperature problem. Allowance does not restore strength.

Then Check Pressure

Class is not independent of material. The same class number gives different allowable pressures for carbon steel, alloy steel and stainless steel. A higher-strength grade can meet the design pressure in a lower class, but only after the table for that group confirms it.

Chrome-moly earns its place where carbon steel would be down-rated. The ASTM A182 F22 alloy steel flanges are the usual example for higher temperature and for hydrogen service. Hydrogen adds its own material and welding rules. F22 on the drawing does not by itself satisfy them.

Then Check the Media

Corrosion overrides both of the screens above. Carbon steel with a corrosion allowance is normal for many hydrocarbons. It is the wrong answer for wet chlorides, acids and seawater.

Type 304 is the general stainless step. Type 316 adds molybdenum and is the step for chloride pitting. Neither is a reliable answer to chloride stress-corrosion cracking. Duplex grades are specified there, and the duplex 2205 flanges are the common choice before super duplex. Confirm the chloride level, the temperature and the oxygen, because duplex has its own limits and is not a universal upgrade.

Strong acids, caustic at high temperature and some sour conditions move past stainless and duplex into nickel alloys. That is a separate selection, made from corrosion data for the alloy, not from the flange class.

Standards, Certificates and Sour Service

ASTM material specifications and the ASME flange standards use related grade names, but the flange standard is what sets dimensions and ratings. EN 1092-1 uses a different designation system. A European grade that looks similar is not automatically the ASME grade. Ask for the equivalent in writing.

The material test report has to match the heat number on the flange. Low-temperature orders need the impact results. Sour service specified to NACE MR0175 / ISO 15156 needs the hardness and heat treatment that document requires. Say so on the order, or the certificate will arrive without those lines.

What Not to Do

  • Do not pick the grade from price and then check whether the service happens to fit.
  • Do not mix carbon steel, stainless and alloy in one bolted joint without checking galvanic corrosion and the gasket.
  • Do not assume a weldable grade is weldable without preheat or post-weld heat treatment. F11, F22 and F91 normally need both.
  • Do not describe a grade as suitable for "all chemicals" or "any temperature."

What to Confirm with Your Inquiry

Give the design temperature, the design pressure, the media, and the material specification you believe applies. Add the flange type, size and facing, and the certificate or test the project requires. The grade is confirmed against all three screens before it is ordered, not after it arrives.

Frequently Asked Questions

When is carbon steel enough for a flange?

Carbon steel suits many non-corrosive services when the pressure-temperature rating is adequate.

When should stainless steel be selected?

Select stainless steel when the media, cleaning chemicals or external environment require corrosion resistance.

Related Products

View More
Call UsWhatsAppEmailInquiry