A flange gasket seals only if the facing, the temperature, the pressure class and the media all suit that gasket. Start with the facing. A sheet gasket, a spiral-wound gasket and a metal ring are not substitutes for each other, and a gasket that is right for the media can still be wrong for the flange.
How a Flange Gasket Seals
Bolt load compresses the gasket into the imperfections of the two faces. The load has to be high enough to close leak paths and low enough not to crush the gasket or bend the flange. The gasket also has to keep sealing while the joint moves with temperature and pressure. That is a requirement on the gasket type, not a property you can add later by tightening harder.
Non-Metallic Gaskets
Non-metallic gaskets are cut from sheet. Rubber, PTFE, flexible graphite and compressed non-asbestos fiber are the usual families. They suit lower pressure and, depending on the sheet, moderate temperature. They are also the gaskets most likely to blow out if the flange class or the facing is wrong.
Do not treat a published temperature as a rating for every brand in that family. Elastomer grades differ from each other, PTFE and graphite depend on the filler and the construction, and the limit that matters is the one on the gasket maker's data sheet for that style. Use the families below as a selection screen, then confirm the sheet.
| Family | What it is for | What to confirm |
|---|---|---|
| Elastomer (NBR, EPDM and others) | Low pressure, where the rubber suits the media | Which rubber, and the maker's temperature limit |
| PTFE | Aggressive chemicals that attack rubber and fiber | Whether it is virgin, filled or expanded |
| Flexible graphite | Higher temperature than rubber or PTFE sheet | Oxidizing media, which graphite does not like |
| Compressed non-asbestos fiber | General moderate service | The binder and the maker's pressure class |
Semi-Metallic Gaskets
Semi-metallic gaskets put a soft filler on a metal carrier, so they hold together at pressures and temperatures that destroy a plain sheet.
- A spiral-wound gasket winds metal strip and filler together. Inner and outer rings center it and stop it being crushed flat. This is the common gasket on raised-face flanges in process plant.
- A metal-jacketed gasket wraps a soft filler in a metal shell.
- A kammprofile, also called a camprofile, is a grooved metal core with graphite or PTFE on the faces.
The metal in the winding or the core has to suit the media, and the filler has to suit the temperature. Specifying "spiral wound" without the metal, the filler and the rings leaves the gasket undefined.
Metallic Gaskets
A ring-joint gasket is a solid metal ring that sits in a ring-type-joint groove and deforms into the groove as the bolts are tightened. Oval and octagonal rings are not interchangeable. The ring and the groove are machined as a pair.
The ring has to be softer than the flange face, or it damages the groove, and it has to resist the media. The Alloy 825 oval ring joint gasket to ASME B16.20 is one example of a ring specified by alloy and by the dimensional standard, which is the level of detail a metallic gasket needs.
A solid flat metal gasket is a different item, used at extreme temperature or pressure. It also has to be softer than the faces it seals against.
Matching the Gasket to the Facing
A full-face sheet belongs on a flat-face flange. A ring gasket belongs in a ring-joint groove and nowhere else. Spiral-wound and kammprofile gaskets are made for raised faces, with the outer ring sitting outside the sealing plateau. Male-and-female and tongue-and-groove facings need a gasket sized to the recess, not a standard raised-face size.
ASME B16.20 covers dimensions for metallic and spiral-wound gaskets. ASME B16.21 covers non-metallic flat gaskets. The inside and outside diameters have to suit the facing and the bolt circle of the flange size and class being bought. A gasket that is the right material and the wrong size does not seal.
What the Gasket Maker Still Has to Confirm
Temperature, pressure and chemical resistance are properties of a construction, not of a family name. Take the short list from this page, then check the data sheet for the style you will buy. If the data sheet does not cover the design temperature, the design pressure and the media, that gasket is not selected yet.
Installing the Gasket You Selected
Clean both faces and reject a face that is scored across the sealing width. Center the gasket and tighten in a cross pattern so it compresses evenly. Do not reuse a crushed gasket. A spiral-wound gasket that has been flattened, or a ring that has already been deformed into a groove, has done its job once.
What to Confirm with Your Inquiry
Give the flange standard, size, class and facing, the design temperature and pressure, and the media. Name the gasket construction, the metal and filler where there is one, the thickness, and whether inner and outer rings are required. Ask for the data sheet that covers those conditions rather than a family name alone.