Product Description
Duplex steel coil is flat-rolled stainless steel supplied in wound form, produced from grades with a mixed austenite-ferrite microstructure. The standard grade on this page is 2205 (UNS S31803 / S32205, EN 1.4462); the lean duplex grade 2304 (UNS S32304, EN 1.4362) and the super duplex grade 2507 (UNS S32750, EN 1.4410) are also supplied in coil form. Coil is the form buyers choose when they need continuous length for roll forming, slitting, pressing, or welding into pipe, tanks and vessel shells.
Against austenitic 304/316 coil, the two-phase structure gives higher yield strength and better resistance to chloride pitting and stress corrosion cracking. What the material actually delivers depends on the grade, the thickness, the surface condition and the service environment - chloride content, temperature, pH, flow rate and whether the surface is flushed or stagnant - so the operating conditions belong on the enquiry instead of being assumed.
Specifications
Supply specification (dimensions confirmed at quotation)
| Item | Value | Status |
|---|---|---|
| Product form | Duplex stainless steel coil. Slit strip and cut-to-length are separate supply options; coil, strip and plate/sheet are different product forms. | Confirmed |
| Grade | 2205 (UNS S31803 / S32205, EN 1.4462); 2304 (S32304, EN 1.4362) and 2507 (S32750, EN 1.4410) also supplied in coil form | Confirmed supply range |
| Standards | ASTM A240/A240M, ASME SA240/SA240M; EN 10088-2; ASTM A480/A480M for general requirements | Reference |
| Condition | Hot rolled and/or cold rolled, solution annealed and pickled - to be confirmed for the ordered thickness | To be confirmed |
| Thickness | Up to 15 mm, subject to confirmation for the ordered grade and width | Confirmed maximum |
| Width | Slit width 50-1500 mm. The minimum width after slitting is 50 mm; availability at the ordered thickness is confirmed with the order. | Confirmed range |
| Length / coil build | Supplied in coil. Cut-to-length, coil weight and coil inner/outer diameter to be confirmed at quotation. | To be confirmed |
| Finish | 2B, 2D, BA, No.1, No.4, HL and pickled, subject to the ordered grade and thickness; other finishes on request | Confirmed options |
| Edge | Mill edge or slit edge | Confirmed options |
| Tolerance | Thickness and width tolerances to be agreed (commonly ASTM A480/A480M or EN 10088-2) | To be confirmed |
| Certification | Mill test certificate to EN 10204 3.1; EN 10204 3.2 where third-party inspection is specified | Confirmed capability |
| Third-party inspection | Available on request - buyer-nominated or mutually agreed inspector; scope, tests and witness points agreed on the order | Confirmed capability |
| Tensile strength (min, ASTM A240) | 620 MPa (90 ksi) for UNS S31803; 655 MPa (95 ksi) for UNS S32205 | Standard reference minimum |
| Yield strength (min, 0.2% offset, ASTM A240) | 450 MPa (65 ksi) for 2205 | Standard reference minimum |
| Elongation (min, ASTM A240) | 25% for 2205 | Standard reference minimum |
| Hardness (2205) | 293 HBW or 31 HRC maximum | Reference |
| Pitting resistance | PREN 34.1 to 37.8 for UNS S32205, calculated as %Cr + 3.3 x %Mo + 16 x %N from the printed S32205 range; the wider UNS S31803 range can fall below 34. Real pitting resistance depends on the service conditions | Calculated reference |
Thickness up to 15 mm and slit widths from 50 mm to 1500 mm are the confirmed supply envelope; the exact gauge, width and tolerance are fixed on the order. Grades 2205, 2304 and 2507, the finishes listed above, and mill certification with optional third-party inspection are confirmed supply capabilities, not stock promises - availability for a given gauge and quantity is answered on the enquiry.
Reference chemical composition, wt% (2205, 2304, 2507)
| Grade | C | Mn | P | S | Si | Cr | Ni | Mo | N |
|---|---|---|---|---|---|---|---|---|---|
| 2205 S31803 | 0.030 max | 2.00 max | 0.030 max | 0.020 max | 1.00 max | 21.0-23.0 | 4.5-6.5 | 2.5-3.5 | 0.08-0.20 |
| 2205 S32205 | 0.030 max | 2.00 max | 0.030 max | 0.020 max | 1.00 max | 22.0-23.0 | 4.5-6.5 | 3.0-3.5 | 0.14-0.20 |
| 2304 (S32304) | 0.03 max | 2.50 max | 0.035 max | 0.020 max | 1.00 max | 21.0-24.0 | 3.50-5.50 | 0.05-0.60 | 0.05-0.20 |
| 2507 (S32750) | 0.03 max | 1.20 max | 0.035 max | 0.020 max | 0.80 max | 24.0-26.0 | 6.00-8.00 | 3.00-5.00 | 0.24-0.32 |
Composition limits are reference values from a supplier datasheet; the limits on your order follow the standard edition and the mill certificate. 904L is sometimes listed alongside duplex grades on supplier pages but is an austenitic grade, not a duplex grade.
Reference mechanical properties at room temperature
| Grade | Tensile strength | Yield strength (0.2% offset) | Elongation | Hardness |
|---|---|---|---|---|
| 2205 S31803 | 620 MPa min | 450 MPa min | 25% min | 293 HBW or 31 HRC max |
| 2205 S32205 | 655 MPa min | 450 MPa min | 25% min | 293 HBW or 31 HRC max |
| 2304 | 600 MPa min | 400 MPa min | 25% min | 293 HBW or 31 HRC max |
| 2507 | 800 MPa min | 550 MPa min | 15% min | 32 HRC max |
These are minimum values published by a supplier for the grade, not measured values for a specific coil. Confirm the required values against the mill certificate for the delivered heat.
Material Characteristics
The ferritic phase raises strength and resistance to stress corrosion cracking, while the austenitic phase keeps toughness and weldability. For a designer this usually means a higher allowable stress than 304/316 coil, and in some cases a reduced gauge for the same load - but the downgauging has to come out of your own calculation and the applicable design code, not out of this page.
Forming behaves differently from austenitic coil. The higher yield strength and lower elongation mean higher forming forces, more springback and a larger minimum bend radius; deep drawing and tight radii should be discussed before the order is placed. Welding is routine with a matching filler (2209 type for 2205) and controlled heat input and interpass temperature, because heat input controls the ferrite-austenite balance in the weld and the heat-affected zone. Follow the qualified welding procedure rather than a generic setting.
Duplex grades also have an upper service temperature limit set by phase stability, including sigma phase and 475 °C embrittlement, and they are not a like-for-like substitute for austenitic grades at high temperature. If the design temperature is high, or the chloride load is severe, tell us the conditions so that 2205, a super duplex grade or an austenitic grade can be compared on the actual duty instead of on the grade name.
Applications
- Oil and gas - process piping, separators, vessel shells and structural components handling chloride-containing produced water.
- Desalination and water treatment - RO pressure vessels, brine handling, piping and tank shells.
- Chemical and petrochemical processing - tanks, scrubbers, heat exchanger shells and process lines.
- Marine and offshore - topside piping, firewater systems and structural fabrications exposed to salt-laden atmospheres.
- Pulp and paper - digester and bleaching equipment where chloride corrosion and strength are both relevant.
Suitability in every case depends on chloride level, temperature, pH, flow and the design code, so the duty should be stated on the enquiry. For flat product in discrete lengths rather than coil, see duplex stainless steel plate and sheet; for the grade-specific coil page, see 2205 duplex stainless steel coil.
Ordering Information
Duplex coil is quoted against the order, not against a stock list, so the enquiry should carry the following:
- Grade and UNS number, and the standard edition you are buying to (ASTM A240/A240M, ASME SA240/SA240M, EN 10088-2).
- Thickness up to 15 mm with tolerance, width 50-1500 mm by slitting with tolerance, and edge condition - mill edge or slit edge.
- Surface finish (2B, 2D, BA, No.1, No.4, HL, pickled or other) and the required supply condition.
- Coil build: coil weight, inner and outer diameter, maximum lift, or the cut lengths if you want cut-to-length sheet.
- Quantity, delivery schedule, packing and destination.
- Service conditions - medium, chloride content, temperature, pH, flow - where corrosion performance drives the grade choice.
- Inspection and documentation: mill test certificate to EN 10204 3.1, or EN 10204 3.2 with third-party or buyer-nominated inspection - state the required tests, witness points and certificate type.
Compare this item with the stainless steel coil range before fixing grade, size and quantity.