254 SMO Tube and Pipe, UNS S31254

254 SMO Tube and Pipe, UNS S31254

254 SMO tube and pipe is UNS S31254 superaustenitic stainless, also called 6Mo or EN 1.4547. It is not a duplex grade. Tube is ordered by OD and wall; pipe is ordered to ASTM A312 by NPS and schedule. Confirm the standard, seamless or welded route, size, and condition with the order.

Grade
254 SMO / Alloy 254, UNS S31254, EN 1.4547
Family
Superaustenitic stainless; EN 10088-2 flat-product limits Cr 19.5–20.5%, Ni 17.5–18.5%, Mo 6.0–7.0%, not a pipe heat analysis and not a guaranteed heat from this page
Product form
Round tube; seamless or welded only as ordered
Pipe standards
ASTM A312 / ASME SA312 when the order is pipe
Tube standards
ASTM A213 or A269 only when the order names them
Size and condition
OD, wall, length, and anneal confirmed per order

Product Description

254 SMO tube is a superaustenitic stainless tube in UNS S31254, also sold as Alloy 254, 6Mo, and EN 1.4547 (X1CrNiMoCuN20-18-7). EN 10088-2 gives the flat-product window as chromium 19.5–20.5%, nickel 17.5–18.5%, and molybdenum 6.0–7.0%, with a deliberate nitrogen addition and a copper addition in the European composition. That window is a flat-product limit, not a pipe heat analysis and not a guaranteed heat from this page. That balance is chosen for chloride pitting and crevice corrosion, not for the strength of a duplex steel.

This page sells both round tube and ASTM A312 / ASME SA312 pipe. Tube is ordered by outside diameter and wall to the tube standard named on the drawing. Pipe is ordered by NPS and schedule. A312 does not by itself make a heat-exchanger tube, an instrumentation tube, or a square hollow section, and a tube order is not filled as pipe.

S31254 is fully austenitic. ASTM A312 does not cover electric-resistance-welded or electric-fusion-welded pipe. B163 and B167 are nickel-alloy tube and pipe standards, not the standard for 254 SMO.

Specifications

The rows below are ordering decisions, not a stock range. Chemistry and strength belong to the product standard and the delivery condition named on the order. A single catalog tensile or yield figure is not a property of every S31254 tube.

ItemHow it is specifiedWhat to confirm
GradeUNS S31254; trade names 254 SMO and Alloy 254; EN 1.4547Which designation the drawing and the certificate must show
FamilySuperaustenitic stainless steel, commonly called 6MoNot duplex, not a nickel-base alloy, not 904L
Product formRound tube on this pageSquare, rectangular, and hydraulic shapes are a different order
ManufactureSeamless or welded, only as the cited standard allowsDo not write ERW or EFW against ASTM A312
Pipe calloutASTM A312 / ASME SA312 when the item is pipeNPS, schedule or wall, and seamless or welded
Tube calloutASTM A213 for seamless heat-exchanger and condenser tube; ASTM A269 for general-service tubeUse the standard the drawing names, not a list of all three
European calloutEN 10216-5 for seamless pressure tube, or the EN tube standard the order citesGrade 1.4547 under that standard, not an assumed ASTM equivalent
SizeTube by outside diameter and wall; pipe by NPS and scheduleNo catalog OD or wall envelope replaces the drawing
ConditionSolution annealed and quenched, as the product standard requiresAnnealing temperature and quench are mill practice under that standard
DocumentsChemical analysis and the tests required by the cited standardEN 10204 3.1 or 3.2, and any third-party inspection, only if the order asks for them

Material Characteristics

EN 10088-2 gives the flat-product composition of 1.4547 as carbon 0.02% maximum, silicon 0.70% maximum, manganese 1.00% maximum, phosphorus 0.030% maximum, sulfur 0.010% maximum, chromium 19.5–20.5%, nickel 17.5–18.5%, molybdenum 6.0–7.0%, nitrogen 0.18–0.25%, and copper 0.50–1.00%. That table is the European flat-product limit, not a pipe heat analysis and not a guaranteed heat from this page. The order and the material certificate govern the heat. A supplier table that prints single “typical” numbers such as 20, 18, 6.1, and 0.7, without minimum and maximum, is not a substitute for those limits.

The same European record classifies 1.4547 as a special austenitic stainless steel and lists UNS S31254 as the reference US designation. It is not a duplex microstructure. Duplex and super duplex grades, including 2205 and 2507, are a different family with a different strength level. 254 SMO is used where a 6% molybdenum austenitic grade is specified. It is not a cheaper copy of 2507, and 2507 is not a substitute unless the drawing allows the change.

Pitting resistance is discussed with a PREN calculated from chromium, molybdenum, and nitrogen. Published PREN formulas are not identical: one common form uses 16 times nitrogen, another uses 30 times nitrogen. Either way, the high molybdenum and the nitrogen addition put S31254 in the same broad class as super duplex for chloride pitting, often described as PREN above 40. That comparison is a screening aid. It is not a corrosion allowance, a seawater guarantee, or a license to skip the medium, temperature, and crevice geometry.

Strength is also standard-specific. Annealed austenitic 6Mo tube is not in the strength class of super duplex. Flat-product data for 1.4547 in the solution-annealed condition are commonly reported with a 0.2% proof strength around 300 MPa and tensile strength in a 650–850 MPa band, with elongation depending on product form and test direction. Those figures are not ASTM A312 pipe minima and are not reprinted here as a guarantee. Ask for the mechanical table in the edition of A312, A213, or A269 named on the order.

Welding needs a matching or over-alloyed consumable and a procedure qualified for this grade. A weld is not automatically more corrosion resistant than the parent metal. Post-weld heat treatment is not forbidden and not automatic; it is specified only when the drawing or the fabrication code requires it. ASTM B163, B167, and AMS 5580 do not apply to this tube.

Applications

Buyers specify S31254 tube and pipe for seawater and brine coolers, ballast and firewater lines, flue-gas cleaning and scrubber duty, bleach plants, and other chloride process equipment where 316L or 904L is no longer enough on pitting. Suitability still depends on temperature, chloride level, crevices, and whether the line is pipe or a heat-exchanger tube.

Do not use this page for boiler tube, a nickel-alloy exchanger tube, a copper-nickel seawater tube, or a super duplex pipe. Those products follow different UNS numbers and different standards. For a higher-molybdenum nickel alloy, see Hastelloy C276 seamless pipe and Hastelloy C22 tube. For 90/10 copper-nickel tube, see C70600 tube. None of those is a drop-in replacement for UNS S31254.

Ordering Information

Send the drawing callouts rather than a catalog size range. The items that change both the product and the quotation are:

  • UNS S31254, 254 SMO, or EN 1.4547, and which name must appear on the certificate
  • Pipe or tube, and the standard: ASTM A312 / ASME SA312, ASTM A213, ASTM A269, EN 10216-5, or another named standard
  • Seamless or welded, using only a route that standard allows
  • Outside diameter and wall for tube, or NPS and schedule for pipe, plus length and quantity
  • Solution-annealed condition, ends, and any supplementary tolerance or corrosion test
  • Inspection documents, including EN 10204 3.1 or 3.2 if required

Working pressure and temperature belong to the piping or exchanger design. This page is not a pressure rating.

Frequently Asked Questions

Is 254 SMO the same as duplex or super duplex?

No. UNS S31254 / EN 1.4547 is a superaustenitic stainless steel, often called 6Mo. Super duplex grades such as UNS S32750 are a different family, with higher strength and their own standards. A PREN comparison does not make the grades interchangeable.

Does ASTM A312 cover this tube?

ASTM A312 covers austenitic stainless steel pipe, seamless, welded, and heavily cold worked. It does not cover ERW or EFW pipe, and it is not the heat-exchanger tube specification. Order tube to ASTM A213 or ASTM A269, or to the EN tube standard on the drawing. Order pipe to ASTM A312 only when the item is pipe.

Can ASTM B163 or B167 be used for 254 SMO?

No. Those are nickel and nickel-alloy tube and pipe standards. 254 SMO is stainless UNS S31254. A nickel-alloy standard number on an old quote does not describe this grade.

What should a quotation request include?

Include the grade name, pipe or tube, the ASTM or EN standard, seamless or welded, outside diameter and wall or NPS and schedule, length, quantity, anneal, ends, supplementary tests, and the inspection documents you need. Availability is confirmed against that request.