ASTM A335 P11 seamless chrome moly pipe (UNS K11597, 1.25Cr-0.5Mo) supplied normalized and tempered for boiler headers, superheater, economiser and intermediate-pressure steam lines. Confirm size, schedule and documentation.

Standard
ASTM A335 / ASME SA-335, Grade P11 (UNS K11597)
Product Form
Seamless pipe, hot finished or cold drawn
Size Range
NPS 1/8" to 24"
Wall Thickness
Schedule number, or specified wall thickness per order
Heat Treatment
Normalized and tempered, or full / isothermal annealed
Ends
Plain end (PE) or beveled end (BE)

Product Description

ASME SA-335 / ASTM A335 Grade P11 is a seamless ferritic chrome molybdenum (chrome moly) alloy steel pipe containing nominally 1.25% chromium and 0.5% molybdenum, UNS K11597. It covers the intermediate-temperature band of steam and process piping — the range where carbon steel has run out of creep strength and oxidation resistance, but the higher 2.25Cr and 9Cr grades are not yet justified. A335 P11 pipe is supplied in the normalized and tempered condition and is suitable for bending, flanging and fusion welding.

Chromium at 1.00–1.50% builds a protective oxide scale that resists scaling in steam and hot gas, while molybdenum at 0.44–0.65% raises creep strength and resists softening under sustained load at temperature. That combination is why P11 is specified for hot steam and hot hydrocarbon service where plain carbon steel would creep and scale. Service limits are not a fixed property of the pipe alone: the allowable stress at temperature is read from the applicable code — ASME BPVC Section II Part D with design to ASME B31.1 or B31.3, or EN 13480 with EN 10216-2 for European projects.

Chemical Composition and Mechanical Properties

The tables below give the ASTM A335 Grade P11 chemical limits and the minimum room-temperature tensile requirements. Values are the standard requirements for Grade P11 — confirm the edition and any supplementary requirements on the purchase order.

ElementASTM A335 Grade P11, heat analysis, %
Carbon (C)0.05–0.15
Manganese (Mn)0.30–0.60
Phosphorus (P)0.025 max
Sulfur (S)0.025 max
Silicon (Si)0.50–1.00
Chromium (Cr)1.00–1.50
Molybdenum (Mo)0.44–0.65

Tensile requirements apply to the 2 in. (50 mm) gauge length unless a 4D proportional specimen is used; elongation therefore depends on the test direction and on wall thickness.

PropertyASTM A335 Grade P11 minimum
Tensile strength415 MPa (60 ksi)
Yield strength, 0.2% offset205 MPa (30 ksi)
Elongation in 2 in. (50 mm), longitudinal30%
Elongation in 2 in. (50 mm), transverse20%

Heat Treatment and Delivery Condition

A335 pipe is heat treated to one of the conditions below. On the normalized and tempered route the tempering temperature is not lower than 650 °C (1200 °F).

ItemRequirement
Normalizing and temperingNormalize at a mill practice of 900–950 °C, which is not an ASTM A335 requirement, then temper at not less than 650 °C (1200 °F)
Annealing alternativesFull anneal or isothermal anneal is also permitted
Usual delivery conditionNormalized and tempered; state any other condition on the order
ASME P-NumberP-No. 4

Dimensional Tolerances

Outside diameter and wall thickness tolerances follow ASTM A335 with reference to ASME B36.10M. The tables below are the standard permissible variations.

NPS designatorOverUnder
1/8 to 1 1/2, incl.0.40 mm (1/64 in.)0.40 mm (1/64 in.)
Over 1 1/2 to 4, incl.0.79 mm (1/32 in.)0.79 mm (1/32 in.)
Over 4 to 8, incl.1.59 mm (1/16 in.)0.79 mm (1/32 in.)
Over 8 to 12, incl.2.38 mm (3/32 in.)0.79 mm (1/32 in.)
Over 12±1% of specified outside diameter—

Permissible variation in wall thickness is quoted as a percentage of the specified wall thickness and depends on the size range and the thickness-to-diameter (t/D) ratio.

NPS designatorOverUnder
1/8 to 2 1/2, all t/D ratios20.0%12.5%
Above 2 1/2, t/D ≤ 5%22.5%12.5%
Above 2 1/2, t/D > 5%15.0%12.5%

Equivalent Grades and Matching Product Forms

P11 is cross-referenced across the main international designation systems and is produced in several matching product forms. These are commonly quoted working references — confirm the property requirements of the governing standard before substituting one designation for another.

SystemDesignation
UNSK11597
EN 10216-213CrMo4-5, material number 1.7335
DIN 1717513CrMo44
JIS G3458STPA 23
GOST 550-7515KhM

The same 1.25Cr-0.5Mo chemistry appears in other product forms under their own standards, so pipe, tube, fittings and plate are not covered by one specification.

Product formStandard
Seamless pipeASTM A335 / ASME SA-335 — this page
Seamless tube for heat exchangersASTM A213 T11
Forged and bored pipeASTM A369 FP11
Forged fittings and flangesASTM A182 F11
Wrought butt-welding fittingsASTM A234 WP11
Plate and sheetASTM A387 Grade 11

Applications

Typical service for A335 P11 pipe is elevated-temperature steam and hot process piping:

  • Boiler headers and manifolds — HP/IP header stub connections and thick-wall manifolds
  • Economiser inlet and outlet headers and connecting lines
  • Intermediate-pressure and hot reheat steam lines
  • HRSG evaporator and superheater headers
  • Refinery and petrochemical elevated-temperature process piping where 1.25Cr-0.5Mo is the specified class

P11 vs P22 vs P91: Grade Selection

Grade selection is driven by metal temperature and creep duty rather than by pressure alone. The table below summarises how the three common chrome moly grades differ.

GradeNominal composition (UNS)Typical roleKey difference
P111.25Cr-0.5Mo (K11597)Intermediate-temperature steam and process piping; headers, economiser and IP steam linesLowest alloy of the three; easiest to weld and post-weld heat treat
P222.25Cr-1Mo (K21590)Hotter main steam and hot reheat serviceHigher creep and oxidation resistance than P11
P919Cr-1Mo-V (K91560)Creep-critical supercritical main steamMartensitic; needs controlled cooling and strict post-weld heat treatment

Ordering Information

To quote A335 P11 pipe, please confirm the following:

  • Standard and edition, and grade: ASTM A335 / ASME SA-335 Grade P11
  • Size: NPS and schedule, or outside diameter with specified wall thickness
  • Length: single random, double random, or cut to length
  • Heat treatment condition, and any hardness or impact requirement
  • End finish: plain end or beveled end
  • Tests and documentation: hydrostatic or nondestructive electric test, PMI, mill test certificate to EN 10204 3.1 / 3.2, third-party inspection
  • Quantity and destination

Common Questions about A335 P11 Pipe

What is ASTM A335 P11 pipe used for?

A335 P11 is specified for elevated-temperature steam and hot process piping: boiler headers and manifolds, economiser connections, intermediate-pressure and hot reheat steam lines, HRSG headers, and high-temperature refinery and petrochemical services. It is chosen where carbon steel has run out of creep strength and oxidation resistance but the higher 2.25Cr or 9Cr grades are not yet required.

What is the difference between P11 and P22?

P11 is nominally 1.25Cr-0.5Mo (UNS K11597) and P22 is nominally 2.25Cr-1Mo (UNS K21590). P22 has higher creep and oxidation resistance for hotter main steam and hot reheat duties, while P11 is the intermediate-temperature grade and is generally easier to weld and post-weld heat treat. They are not interchangeable without re-checking the allowable stress at the design temperature.

In what condition is A335 P11 pipe supplied?

Normalized and tempered is the usual delivery condition, with a tempering temperature of not less than 650 °C (1200 °F). Full annealing or isothermal annealing is also permitted by the specification. State the required condition, and any hardness or impact requirement, on the purchase order.

Is a hardness test mandatory for A335 P11?

No. ASTM A335 does not make hardness testing a mandatory acceptance test for Grade P11; the hardness limit printed in the specification applies to Grade P91. Some data sheets quote a Brinell ceiling for P11, but published values disagree with each other, and a hardness cap is normally imposed only by a project specification or by sour-service requirements such as NACE MR0175 / ISO 15156. Specify the limit you need on the order.

How should P11 be welded?

P11 is a ferritic chrome moly steel and should not be welded like carbon steel. It requires controlled preheat, matching 1.25Cr-0.5Mo filler metal (ER80S-B2 / B2 class), and post-weld heat treatment in accordance with the applicable code and the approved welding procedure. The post-weld heat treatment temperature and holding time are set by the code and the wall thickness, so take them from the approved WPS rather than a generic figure.

This page covers A335 P11 seamless pipe only. Browse the Alloy Steel Pipe range for the wider chrome moly family, or compare with WB36 alloy pipe, a different power-plant alloy based on copper-nickel precipitation rather than chromium. The same 1.25Cr-0.5Mo chemistry in plate form is covered by ASTM A387 Grade 11 chrome moly steel plate. For material selection across stainless, nickel and alloy piping, start from stainless steel, nickel and alloy piping.

You Might Also Like

View More
Call UsWhatsAppEmailInquiry