Skip to Content
Hastelloy C22 (UNS N06022) Seamless Tube

Hastelloy C22 (UNS N06022) Seamless Tube

Hastelloy C22 (UNS N06022, DIN 2.4602) seamless tube in the solution-annealed condition to ASTM B622 / ASME SB622, for service in mixed oxidizing and reducing corrosive media. Sizes and lengths confirmed per order.

Product Form
Seamless tube; ASTM B622 also covers seamless pipe sizes
Grade / Trade Names
Hastelloy C22 / Alloy 22 (Ni-Cr-Mo-W corrosion-resistant alloy)
UNS / W.Nr.
N06022 / DIN 2.4602 (EN NiCr21Mo14W)
Standard
ASTM B622 / ASME SB622 — Seamless Nickel and Nickel-Alloy Pipe and Tube
Condition
Solution annealed, rapidly cooled (usual anneal target 1121 °C / 2050 °F, not a B622 acceptance item)
Size (OD × Wall)
To be confirmed per order — submit OD and wall thickness or NB plus schedule

Product Description

Hastelloy C22 seamless tube — also known as Alloy 22, UNS N06022, or DIN 2.4602 (NiCr21Mo14W) — is a nickel-chromium-molybdenum-tungsten corrosion-resistant alloy supplied in the solution-annealed condition to ASTM B622 / ASME SB622. The grade combines high chromium (20.0–22.5 %) with molybdenum (12.5–14.5 %) and tungsten (2.5–3.5 %), so it withstands both oxidizing and reducing corrosive media, including media that swing between the two during process upsets.

Typical selection drivers are pitting, crevice corrosion and stress-corrosion-cracking resistance in wet chlorine, hypochlorite and chlorine dioxide environments, ferric and cupric chlorides, acetic and formic acids, seawater and brine, and contaminated mixed-acid streams. Actual performance always depends on concentration, temperature and impurity levels in your service, so share the medium details when requesting a quotation.

Chemical Composition

The limits below are the UNS N06022 composition applied by ASTM B622 for seamless product, expressed in weight percent.

ElementContent (wt %)
Nickel (Ni)Balance
Chromium (Cr)20.0–22.5
Molybdenum (Mo)12.5–14.5
Tungsten (W)2.5–3.5
Iron (Fe)2.0–6.0
Cobalt (Co)≤2.5
Carbon (C)≤0.015
Manganese (Mn)≤0.50
Silicon (Si)≤0.08
Vanadium (V)≤0.35
Phosphorus (P)≤0.020
Sulfur (S)≤0.020

Some supplier compilations list carbon as 0.010 % maximum; the UNS N06022 limit is 0.015 % maximum, which is the value published here.

Mechanical Properties

The values below are the minimum room-temperature requirements for annealed UNS N06022 seamless pipe and tube under ASTM B622.

PropertyMinimum (annealed)
Tensile strength690 MPa (100 ksi)
Yield strength, 0.2 % offset310 MPa (45 ksi)
Elongation in 2 in.45 %

Welded C22 products (B619 welded pipe, B626 welded tube, B474 electric-fusion-welded pipe) are specified and tested to their own standards, and some compilations quote 283 MPa yield or 40 % elongation — those figures belong to welded construction, not to this seamless tube. Reference physical properties of the alloy: density 8.69 g/cm³ (0.314 lb/in³) and melting range 1,357–1,399 °C (2,475–2,550 °F).

Material Characteristics

C22 is one of the few nickel alloys that resists grain-boundary precipitate formation in the weld heat-affected zone, which is why the alloy is widely used in the as-welded condition and post-weld heat treatment is normally not required. Matching filler metal is ERNiCrMo-10; control heat input and clean the weld area as with other high-nickel alloys. The alloy work-hardens during cold forming, so intermediate anneals may be needed for heavy deformation.

The microstructure must stay in the solution-annealed state: the usual anneal target for N06022 is 1121 °C (2050 °F), followed by rapid cooling. That temperature is common practice, not an ASTM B622 acceptance item. Slow cooling through the intermediate-temperature range allows carbide and intermetallic phases to precipitate and reduces both corrosion resistance and ductility, so avoid slow-cooled inventory.

Compared with Hastelloy C-276 seamless pipe, C22 carries noticeably more chromium (20.0–22.5 % versus about 14.5–16.5 %), which makes it the stronger performer in oxidizing media such as wet chlorine gas, hypochlorite and mixed-acid systems, while C-276's higher molybdenum retains an edge in strongly reducing acids such as hot concentrated hydrochloric acid. If your process chemistry varies between oxidizing and reducing conditions, C22 is often the more forgiving choice.

Applications

Seamless C22 tube is specified for chemical processing equipment (reactor coils, heat-exchanger tubing, pickling lines), flue gas desulfurization scrubbers and dampers, chlorination and hypochlorite systems, pharmaceutical and fine-chemical lines where corrosion products must be avoided, seawater cooling and brine handling, and waste-water or waste-incineration scrubber circuits. The grade is also listed in NACE MR0175 / ISO 15156 sour-service material tables; confirm the applicable edition and environmental restrictions for your project before ordering.

C22 is also produced in other product forms for different intents: coil and strip for formed parts (see Hastelloy alloy coil) and plate for vessels. Keep tube, pipe and coil requirements on separate inquiries so each is quoted against the correct standard.

Frequently Asked Questions

Is ASTM B474 a seamless tube standard for Hastelloy C22?

No. ASTM B474 is titled "Standard Specification for Electric Fusion Welded Nickel and Nickel Alloy Pipe"; it covers Class 1–5 welded pipe and its commercial practice is commonly limited to 8 in. nominal diameter and above. It is not a seamless tube specification. Seamless C22 pipe and tube is covered by ASTM B622 / ASME SB622, which is the standard this product is quoted against.

How does Hastelloy C22 compare with C276?

C22 has 20.0–22.5 % chromium versus about 14.5–16.5 % in C276, so C22 performs better in oxidizing media (wet chlorine, hypochlorite, mixed-acid streams), while C276's higher molybdenum (15–17 %) keeps an advantage in strongly reducing acids such as hot concentrated hydrochloric acid. Both are separate products with their own pages; choose by the dominant chemistry of your service.

What information should I include in an inquiry?

Outside diameter and wall thickness (or NB plus schedule), length, quantity, standard (ASTM B622 / ASME SB622), solution-annealed condition, end preparation, the certificate type you need, and the service medium with temperature so corrosion resistance can be checked before quoting.

What mechanical properties are guaranteed for annealed C22 seamless tube?

ASTM B622 requires minimum tensile strength of 690 MPa (100 ksi), 0.2 % offset yield strength of 310 MPa (45 ksi) and elongation of 45 % in 2 in. for annealed N06022 seamless product. Figures such as 283 MPa yield or 40 % elongation found on some websites refer to welded product forms, not seamless tube.

Ordering Information

When requesting a quotation, please provide: quantity; OD × wall thickness (or NB plus schedule); length; the governing standard (ASTM B622 / ASME SB622 or equivalent); condition (solution annealed); end preparation; required documentation such as an EN 10204 3.1 certificate; and, where corrosion resistance needs checking, the medium, concentration and temperature. Sizes and lengths are confirmed per order.

You Might Also Like

View More
Call UsWhatsAppEmailInquiry