Weld Neck Flange: Bore, Hub and Ratings

James Blue, Piping Materials Specialist

Weld Neck Flange: Bore, Hub and Ratings

A weld neck flange has a long tapered hub that carries stress from the pipe wall into the flange ring, and it is attached with a single full-penetration butt weld. Order it by pressure class, size, bore schedule, facing and material: the hub geometry follows the class, it does not set the rating.

What the Hub Does

The hub tapers from the welding end to the flange ring, so the load path from pipe to flange is gradual rather than stepped. That lowers the peak stress at the weld toe and is the reason this type is chosen for high pressure, high temperature and cyclic service. The bore is machined to match the pipe wall, which keeps the flow path smooth and removes the crevice that a socket weld or threaded joint leaves behind.

Dimensions to State on the Order

  • NPS and bore schedule, so the bore matches the pipe wall: NPS 6 Schedule 40 is 168.3 mm outside diameter with a 7.11 mm wall.

  • Pressure class and facing: raised face, ring type joint, or tongue and groove.

  • Welding end preparation, normally to ASME B16.25.

  • Material specification and, where the rating depends on it, the material group.

  • Heat treatment and examination requirements for the finished weld.

Pressure-Temperature Ratings

A rating is not a property of the hub. It comes from the pressure class, the material group and the temperature, read from the tables in ASME B16.5, which covers NPS 1/2 through NPS 24. Confirm the edition on the order and read the rating for the material group you are buying, not for the class alone. Weld neck flanges are produced across the whole class range, which is one reason they are used where slip-on and threaded types fall away.

Materials

Forged carbon steel to ASTM A105 is the general-service choice; see ASTM A105 carbon steel flange. Stainless grades to ASTM A182 F304 and F316 cover corrosive media and are stocked across the common classes; see ASME B16.5 stainless steel flanges. Chrome-moly grades F11 and F22 serve elevated-temperature creep duty, and ASTM A350 LF2 covers low-temperature service. Select the material from the media and the temperature, then confirm the class rating for that material group.

Weld Neck Compared with Slip-On and Socket Weld

FactorWeld neckSlip-onSocket weld
WeldOne full-penetration butt weldTwo fillet weldsOne fillet weld
Stress pathGradual through the tapered hubAbrupt at the flange faceAbrupt, with a root gap inside
Fatigue and cyclingBest of the threeModerateModerate; the crevice can corrode
BoreMachined to the pipe wall, smooth boreBore larger than the pipeBore larger than the pipe
ExaminationRadiography or ultrasonics possibleSurface examinationSurface examination
Cost and fit-upHighest cost, needs alignmentLower cost, easy fit-upLower cost, small-bore only

Welding, Examination and Heat Treatment

Prepare the welding end to ASME B16.25 and match the consumable to the base material so the weld metal properties hold across the joint. Preheat where the procedure calls for it, control the interpass temperature, and record both. Post-weld heat treatment is driven by the construction code and the material thickness, so confirm the requirement against ASME B31.3 rather than assuming it applies.

What to Confirm with Your Inquiry

  • Standard, pressure class and facing

  • Size and bore schedule, or the matching pipe wall thickness

  • Material specification and material group

  • Welding end preparation and any PWHT requirement

  • Examination scope and certificate type

Send the class, size and bore schedule with your inquiry and we will confirm availability and rating.

Frequently Asked Questions

Why does a weld neck flange have a long hub?

The tapered hub spreads stress from the pipe wall into the flange and suits demanding pressure service.

What must match the pipe?

The bore, wall schedule, material and welding end preparation must match the connected pipe.