Skip to Content

Flange Inspection: What to Check Before Use

James Blue, Piping Materials Specialist

Flange Inspection: What to Check Before Use

Flange inspection checks four things on every piece: the sealing face, the dimensions, the marking, and the material certificate that matches the heat number. Ultrasonic, magnetic-particle, penetrant, radiographic and pressure tests are added by the order. They are not included just because a flange was manufactured.

Why the Four Checks Come First

A flange can pass a chemistry test and still leak because the face is scored, or pass a dimensional check and still be the wrong material because the certificate is for a different heat. The four checks catch different failures. Skipping one because another was done leaves that failure in the delivery.

Visual Check

Look at the sealing face under enough light to see a radial score, a dent or corrosion. Damage that crosses the sealing width is a leak path. Look for cracks, laps and seams on the hub and the bore, and confirm the bolt holes are present and not elongated.

Then read the marking. ASME B16.5 requires the manufacturer and the material designation, among other marks. A pressure class, size and heat number are what connect the piece in your hand to the certificate. The ASTM A105 carbon steel flange is a typical piece where that marking is the start of the inspection, not a label to ignore.

Dimensional Check

Measure against the flange standard named on the order, for the stated size and class: outside diameter, thickness, bore, bolt-circle diameter and bolt-hole diameter. On a weld-neck flange, check the hub. On a raised face, check the face height and diameter. On a ring-joint flange, gauge the groove rather than judging it by eye.

Surface finish on the sealing face is a dimensional requirement too. Compare it with the limit in the standard edition the order cites. A finish that is too rough or too smooth for the gasket is a nonconformance even when the diameter is right.

Which NDT Method Finds What

Order only the methods that match the material and the defect you need to find. A method that cannot see the defect you care about is not extra assurance.

MethodWhat it can findWhat it does not cover
VisualFace damage, marking, obvious cracksAnything under the surface
DimensionalWrong size, thickness, bore, grooveMaterial and internal soundness
UltrasonicLaminations and internal discontinuities in forgings and plateA tight surface crack parallel to the beam
Magnetic particleSurface and near-surface cracks in magnetic steelAustenitic stainless and other non-magnetic alloys
Liquid penetrantSurface cracks open to the dyeInternal defects, and any crack that is closed
RadiographyInternal voids in castings and weldsA crack that does not present an edge to the beam
Positive material identificationWhether the alloy family matches the markingA full heat analysis or mechanical properties

Liquid penetrant is the usual surface method for non-magnetic stainless flanges, the group represented by the ASME B16.5 stainless steel flanges. Magnetic particle will not work on that material. Positive material identification is a sorting test. It does not replace the mill certificate.

Pressure Testing

A loose flange is not normally pressure tested by itself. A hydrostatic test checks an assembled joint or a piping system. When ASME B31.3 applies, the test pressure and hold time come from that code and from the design conditions. Do not invent a test pressure by multiplying the class number. A system that cannot be filled with water may use a pneumatic test, which needs its own safety controls and is specified separately.

The Certificate Has to Match the Piece

A material test report states the chemical analysis and the mechanical results for a heat. The heat number stamped on the flange has to be the heat number on the report. A report for a different heat, or a report that does not name the specification on the marking, does not certify the piece.

Low-temperature orders need the impact results the material specification requires. Sour-service orders need the hardness and heat-treatment records the project calls up under NACE MR0175 / ISO 15156. Ask for those pages. A standard test report does not include them unless the order did.

Marking and Traceability

Permanent marking should include the manufacturer, the material designation and enough information to find the certificate. Low-stress stamping matters on flanges that will be highly stressed. The trail behind the stamp runs from the heat to the forging, the heat treatment, the machining and this inspection. If a step in that trail has no record, the flange is not fully traceable, whatever the stamp says.

What to Confirm with Your Inquiry

State the flange standard, size, class, facing and material. List the inspections you want: visual, dimensional, and any NDT with the coverage and the acceptance standard. Name the certificate, such as a material test report or EN 10204 3.1, and add impact, hardness or PMI only if the service requires them. An inspection that is not written into the order will not be on the paperwork.

Frequently Asked Questions

What does flange inspection usually include?

It includes visual checks, dimensions, material identification and the NDT or certificate review required by the order.

Why compare the marking with the certificate?

Heat number, grade and standard markings must trace back to the material test certificate.

Related Products

View More
Call UsWhatsAppEmailInquiry