Low-Temperature Flange Impact Testing

James Blue, Piping Materials Specialist

Low-Temperature Flange Impact Testing

Low-temperature flange selection starts with the minimum design metal temperature and the Charpy V-notch (CVN) impact test condition, not with a single temperature printed beside a grade name. ASTM A350/A350M Grade LF2 defines the material, the heat treatment and the notch toughness requirement. ASME B16.5 or ASME B16.47 defines the size, pressure class, facing and drilling. The two are ordered separately.

What a Low-Temperature Requirement Contains

A low-temperature callout is three decisions made in sequence: the minimum design metal temperature for the line; whether the applicable piping code, in the edition named on the order, requires impact testing at that temperature for the chosen material group; and which material class carries the impact condition the project needs. Where the applicable code permits the selected material without impact testing, ASTM A105 may remain eligible. When the design requires an impact-tested carbon steel forging, A350 LF2 is a candidate whose class must be selected from the required test condition. Where the service falls outside the LF2 conditions, other materials have to be evaluated against the design and governing code rather than assumed from a grade name.

A temperature attached to a grade in a supplier table is usually a test condition, not a service limit. The -50 F [-46 C] figure associated with LF2 is the Charpy test temperature of Class 1 in ASTM A350/A350M. It is not a universal service limit, and it does not replace the code calculation for the line.

Material Standard and Dimensional Standard Do Different Jobs

A350/A350M defines the material only: chemistry, heat treatment, tensile properties and notch toughness. It does not dimension the flange. Dimensions, facings, drilling and pressure class come from ASME B16.5 for NPS 1/2 through NPS 24, or from ASME B16.47 Series A or Series B for NPS 26 through NPS 60. The series letter belongs on the enquiry for any flange above NPS 24, because the two series are not interchangeable on the same bolting.

A961/A961M, the common requirements specification for steel flanges, also applies, and supplementary requirements apply only when they are named on the order.

Class 1 and Class 2 Impact Conditions

Class 1 and Class 2 are the same LF2 material with the same tensile and yield requirements; what separates them is the impact test condition and the absorbed energy required. Both are tested with standard 10 mm by 10 mm Charpy V-notch specimens, with sub-size specimens permitted under the proportional energy table.

ClassTest temperatureAverage of 3 specimens, minOne specimen, min
Class 1-50 F [-46 C]15 ft-lbf [20 J]12 ft-lbf [16 J]
Class 20 F [-18 C]20 ft-lbf [27 J]15 ft-lbf [20 J]

Class 1 is qualified at the colder test temperature with the lower energy requirement; Class 2 is tested at the warmer temperature but has to absorb more energy. Neither is automatically the better buy: the class follows the minimum design metal temperature and the fracture margin the project asks for, and the test temperature on the order should match the condition being qualified. A single minimum impact energy quoted with no class and no test temperature does not identify a requirement, and because the class changes the impact condition rather than the strength level, a table showing a higher minimum yield for Class 2 is describing another material.

Where A105 Stops and LF2 Starts

The two carbon steel forgings share the same minimum tensile and yield values, which is why the choice is so often made on temperature alone. The real difference is the impact test requirement.

ItemA350 LF2A105
Tensile strength70 - 95 ksi [485 - 655 MPa]70 ksi [485 MPa] minimum
Yield strength, min36 ksi [250 MPa]36 ksi [250 MPa]
Impact testingMandatory Charpy V-notch, by classNot required unless named as a supplementary requirement
Heat treatmentNormalized, normalized and tempered, or quenched and temperedNot mandatory in every case; specified when the order or design condition calls for it

LF2 cannot be released without impact test records, so a flange offered without them is being offered to a different specification and should be quoted as such. Neither grade should be described as corrosion resistant; coating or painting is a separate line on the order. The impact test qualifies the forging, not the whole duty: where the fluid is directly on a liquefied gas at temperatures well below the LF2 test range, austenitic stainless or a nickel steel grade is normally the material of record. The full envelope is on the ASTM A350 LF2 low-temperature carbon steel flange page, and the general-service forging on the ASTM A105 carbon steel flange page.

Procurement Checks

Four checks catch most low-temperature ordering errors:

  • Confirm the class and the test temperature on the certificate, not just the grade: Class 1 and Class 2 share one tensile range.
  • Confirm the dimensional standard and the series letter above NPS 24, and read the pressure class separately from the material class.
  • Confirm the heat treatment condition appears on the certificate as ordered; it is part of the requirement, not a mill preference.
  • Confirm the documentation package: certificate type, heat treatment records, impact test results, and any supplementary requirement from A350/A350M or A961/A961M.

Two further checks do not substitute for those above. Positive material identification confirms alloy content and does not qualify an impact test condition. An ASME pressure class is a pressure-temperature rating and dimensional designation, not a material class.

Why do low-temperature flanges need impact tests?

Impact testing demonstrates that the selected material keeps adequate toughness at the design temperature.

Which flange grade is commonly used for low temperature?

ASTM A350 LF2 is a common carbon-steel choice, subject to the project temperature and code requirements.

Frequently Asked Questions

Why do low-temperature flanges need impact tests?

Impact testing demonstrates that the selected material keeps adequate toughness at the design temperature.

Which flange grade is commonly used for low temperature?

ASTM A350 LF2 is a common carbon-steel choice, subject to the project temperature and code requirements.