Skip to Content

Incoloy 825 Seamless Tube Standard Guide

James Blue, Piping Materials Specialist

Incoloy 825 Seamless Tube Standard Guide

Incoloy 825 is a titanium-stabilized nickel-iron-chromium alloy with molybdenum and copper additions, designated UNS N08825 (W.Nr. 2.4858, JIS NCF825). For seamless product it is specified under ASTM B423 for pipe and ASTM B163 for condenser and heat-exchanger tube, and its composition and mechanical minimums are fixed by those standards rather than by supplier claims. This guide collects the acceptance limits buyers check against a mill test certificate.

Chemical Composition of UNS N08825

The table below is the heat-analysis acceptance range for UNS N08825 under the ASTM nickel-alloy specifications; the mill certificate for the delivered heat remains the acceptance document.

ElementContent (% by mass)
Nickel, Ni38 - 46
Chromium, Cr19.5 - 23.5
Iron, Fe22 min (balance)
Molybdenum, Mo2.5 - 3.5
Copper, Cu1.5 - 3.0
Titanium, Ti0.6 - 1.2
Carbon, C0.05 max
Manganese, Mn1.00 max
Silicon, Si0.50 max
Sulfur, S0.03 max
Aluminum, Al0.20 max

Mechanical Minimums in the Annealed Condition

ASTM B423 defines two annealed conditions for UNS N08825 and they carry different mechanical minimums, so the condition must be stated on the order.

ConditionTensile strength, minYield (0.2% offset), minElongation, min
Hot-finished annealed517 MPa (75 ksi)172 MPa (25 ksi)30%
Cold-worked annealed586 MPa (85 ksi)241 MPa (35 ksi)30%

The material cannot be hardened by heat treatment; strength comes from the cold-work level before the final anneal. For sustained structural service the alloy carries a 540 °C reference ceiling, with long-term exposure above that temperature potentially reducing ductility; design stresses come from the ASME Boiler and Pressure Vessel Code Section II-D tables, not from the room-temperature minimums.

Why the Alloy Resists Corrosion

Each element has a defined role. The 38 - 46% nickel stabilizes the austenitic matrix and is what separates 825 from standard austenitic stainless steels under chloride stress-corrosion cracking. The 19.5 - 23.5% chromium provides resistance to oxidizing media such as nitric acid. The 2.5 - 3.5% molybdenum improves pitting and crevice performance in chloride-bearing waters, while the 1.5 - 3.0% copper extends resistance into the reducing acid domain (sulfuric and phosphoric) where stainless steels are borderline. The 0.6 - 1.2% titanium ties up carbon, which is why the alloy is normally used in the as-welded condition without post-weld heat treatment.

Equivalent Grade Designations

RegionDesignation
USAUNS N08825 (Incoloy 825)
Germany / EUW.Nr. 2.4858, EN NiFe30Cr21Mo3CuTi
JapanJIS NCF825

These are cross-system references; the delivered item is supplied against the standard named in the purchase order.

Tube or Pipe: Which Standard Applies

The same UNS chemistry covers several product forms, and each form has its own specification. Condenser and heat-exchanger tube is ordered to ASTM B163 / ASME SB163 with outside-diameter-based tolerances; seamless pipe for process service is ASTM B423 / ASME SB423; welded tube and large-bore welded pipe follow B704 and B705. Confirm the form before requesting a quotation: the Incoloy 825 seamless pipe (UNS N08825) page covers the pipe route, including the NPS-to-outside-diameter chart that catches suppliers who quote nominal inch sizes as if they were millimetre outside diameters.

UNS N08825 is listed in NACE MR0175 for H2S-bearing oil and gas environments, but that document places limits on hardness, environment severity and product form, so sour-service applicability is qualified per project rather than assumed from the grade name.

What to Confirm Before Ordering

A complete inquiry states: the standard and product form (B163 tube or B423 pipe), size (NPS plus schedule, or outside diameter plus wall), length, delivery condition (hot-finished annealed or cold-worked annealed), surface finish, quantity, and the inspection and document package - EN 10204 3.1 or 3.2 mill test certificate, PMI, NDT scope, and NACE MR0175 requirements if the service is sour. Where corrosion duty is dominated by strong reducing acids, compare the alloy against Hastelloy C276 seamless pipe before finalizing the grade.

Frequently Asked Questions

Is Incoloy 825 a nickel alloy or stainless steel?

The guide describes it as a stabilized iron-based austenitic alloy with substantial nickel, chromium and molybdenum additions.

Which product matches an Incoloy 825 tube inquiry?

Use the Incoloy 825 seamless pipe page and confirm UNS designation, size and test requirements on the order.

Related Products

View More
Call UsWhatsAppEmailInquiry