title: "Steel Plate Grades: A36, A516, A572, 304 - Gangyou Steel"
description: Steel plate grades differ by duty. Compare A36, A516 Gr.70, A572 Gr.50, 304 and 2205 by yield strength, impact test temperature and thickness.
image: https://pipemanufactory.com/uploads/images/blog_steel-plate-complete-guide-types-grades-sta-103541.webp
---

# Steel Plate Grades: A36, A516, A572, 304

June 16, 2026 James Blue, Piping Materials Specialist

![Steel Plate Grades: A36, A516, A572, 304](/uploads/images/blog_steel-plate-complete-guide-types-grades-sta-103541.webp)

Plate selection starts with the duty, not the grade name. A structural grade, a pressure-vessel grade, a wear grade and a corrosion-resistant grade answer different questions, and the order has to carry the standard edition, thickness range, heat treatment condition and any impact test requirement. Chemistry alone will not tell you which one you need.

## What Counts as Steel Plate

Plate is flat-rolled product produced by hot rolling slab and cutting to length. A thickness of about 3 mm is a common boundary between sheet and plate, but the boundary is set by the standard or the mill practice in question, so confirm it rather than assuming it. Thickness bands used in practice are roughly 3-20 mm for medium plate, 20-60 mm for thick plate and above 60 mm for extra-thick plate, with the maximum available depending on the mill.

Condition matters as much as grade. As-rolled, normalised, and quenched and tempered plate of the same grade do not have the same properties, and the condition is a line item on the order.

## Carbon Steel Plate Grades

Carbon steel plate carries the largest share of structural and vessel work. The values below are typical minimum mechanical properties quoted against the standard; confirm the edition and the thickness range that applies, because minimum yield usually steps down as thickness increases.

| Grade | Min yield (MPa) | Tensile (MPa) | Typical duty |
| --- | --- | --- | --- |
| ASTM A36 | 250 | 400-550 | General structural work, base plates, frames |
| ASTM A516 Gr.70 | 260 | 485-620 | Pressure vessels and boilers, moderate temperature |
| ASTM A572 Gr.50 | 345 | 450-600 | High-strength structural members, bridges |
| EN S355J2 | 355 | 470-630 | Structural work with -20 degrees C impact requirement |

A36 remains the general structural default where no impact or through-thickness requirement exists. A572 Gr.50 raises minimum yield from 250 MPa to 345 MPa, which is what allows lighter sections. A516 is a different category: it is specified for pressure-containing parts, and it is normally ordered with a stated heat treatment and, where the design requires it, impact testing at a stated temperature. Low-temperature toughness is a supplementary requirement to be named on the order - it is not implied by the grade number. The grades and conditions to ask for are set out on the [ASTM A516 carbon steel plate](/products/steel-plate/hot-rolled-steel-plate/astm-a516-carbon-steel-plate) page.

For non-critical fabrication and general engineering, [low carbon steel plate](/products/steel-plate/hot-rolled-steel-plate/low-carbon-steel-plate) and [Q235 carbon steel plate to GB/T 700](/products/steel-plate/hot-rolled-steel-plate/q235-carbon-steel-plate) are the common commercial options, and the choice between them is usually governed by which standard the drawing calls up. Where a drawing names an EN or GB grade and the mill offers an ASTM equivalent, the same comparison rules apply as for pipe, which are set out in [comparing steel grades across standards](/blog/metal-material-international-standard-equivale-103529130).

## Stainless and Duplex Plate Grades

| Grade | Min yield (MPa) | Key alloying | Typical duty |
| --- | --- | --- | --- |
| 304 / 304L | 205 | 18% Cr, 8% Ni | Food, architectural, general chemical |
| 316 / 316L | 205 | 16% Cr, 10% Ni, 2% Mo | Marine, pharmaceutical, chloride service |
| 2205 duplex | 450 | 22% Cr, 5% Ni, 3% Mo | Chemical and offshore, higher strength |
| 2507 super duplex | 550 | 25% Cr, 7% Ni, 4% Mo | Aggressive chloride and high-pressure service |

Molybdenum is the reason 316 is chosen over 304 in chloride service, and the duplex grades roughly double the yield strength of 304 while improving resistance to chloride stress corrosion cracking. Higher strength comes with tighter welding controls: duplex plate needs a qualified procedure and controlled heat input, so the fabrication route should be settled before the grade is fixed.

Each of these is ordered against its own ASTM specification, and the finish and condition belong on the enquiry: [304 stainless steel plate](/products/steel-plate/stainless-steel-plate/304-stainless-steel-plate), [duplex stainless plate and sheet](/products/steel-plate/stainless-steel-plate/duplex-stainless-steel-plate-and-sheet) and [2507 super duplex plate](/products/steel-plate/stainless-steel-plate/2507-super-duplex-stainless-steel-plate-uns-s32750).

## Alloy and Heat-Resistant Plate

Cr-Mo plate such as [ASTM A387 Grade 11](/products/steel-plate/hot-rolled-steel-plate/astm-a387-grade-11-chrome-moly-steel-plate) is specified for elevated-temperature and hydrogen service, and is usually ordered in the normalised and tempered condition with class stated. Grades such as 310S are chosen for oxidation resistance at high temperature; the temperature a grade can tolerate in air is not the same as its allowable design stress at that temperature, so the design code governs the number that goes on the drawing.

## What to Confirm with Your Inquiry

Plate enquiries come back faster and more accurately when these fields are complete:

- Grade and governing standard with edition, for example ASTM A516 Gr.70 or EN 10028-2 P265GH.
- Thickness, width and length, and whether those are nominal or minimum.
- Heat treatment or delivery condition: as-rolled, normalised, quenched and tempered, solution annealed.
- Impact test temperature and absorbed energy, and whether through-thickness (Z-direction) testing is required.
- Non-destructive testing scope, for example ultrasonic testing to a stated acceptance level.
- Surface condition, edge preparation, and any cutting, bevelling or priming required.
- Quantity in tonnes or pieces, plus the delivery term and destination.

Standards define what a grade must achieve; they do not define what any supplier can offer on a given order. Availability, thickness range, cutting capability and certificate scope all have to be confirmed per order.

## Frequently Asked Questions

### When is ASTM A516 used instead of A36?

A516 is specified for pressure-containing parts such as vessels and boilers, while A36 is a general structural carbon steel grade without a pressure-vessel scope.

### What belongs on a steel plate enquiry?

Grade and standard with edition, thickness, width and length, heat treatment condition, impact test temperature, NDT scope, surface condition and quantity.

Share [Facebook](https://www.facebook.com/sharer/sharer.php?u=https%3A%2F%2Fpipemanufactory.com%2Fblog%2Fsteel-plate-complete-guide-types-grades-sta-103541230) [X](https://twitter.com/intent/tweet?url=https%3A%2F%2Fpipemanufactory.com%2Fblog%2Fsteel-plate-complete-guide-types-grades-sta-103541230) [LinkedIn](https://www.linkedin.com/shareArticle?url=https%3A%2F%2Fpipemanufactory.com%2Fblog%2Fsteel-plate-complete-guide-types-grades-sta-103541230)

[Send Inquiry](/inquiry?ref=steel-plate-complete-guide-types-grades-sta-103541230)

Latest Posts

- [!\[Steel Pipe Lead Time from China Explained\](/uploads/images/blog_steel-pipe-lead-time-from-china-complete-guid-1035.webp) Steel Pipe Lead Time from China Explained](/blog/steel-pipe-lead-time-from-china-complete-guid-103565829)
- [!\[Steel Pipe Export Packaging and Shipping\](/uploads/images/blog_steel-pipe-export-packaging-and-shipping-guide-103.webp) Steel Pipe Export Packaging and Shipping](/blog/steel-pipe-export-packaging-and-shipping-guide-103565688)
- [!\[How to Audit a Chinese Steel Pipe Factory\](/uploads/images/blog_how-to-audit-a-chinese-steel-pipe-factory-com-1035.webp) How to Audit a Chinese Steel Pipe Factory](/blog/how-to-audit-a-chinese-steel-pipe-factory-com-103565697)

## Related Products

[View More](/products)

![2507 Super Duplex Stainless Steel Plate (UNS S32750)](/uploads/images/duplex-steel-plate-sheet-3.webp)

### [2507 Super Duplex Stainless Steel Plate (UNS S32750)](/products/steel-plate/stainless-steel-plate/2507-super-duplex-stainless-steel-plate-uns-s32750)

2507 super duplex stainless steel plate for projects that specify S32750 (2507). S32760 is a related grade with slight elemental differences and must be specified separately. Confirm the requested grade, applicable product standard and dimensions before quotation.

![304L Stainless Steel Plate](/uploads/images/ss304-plate-9.webp)

### [304L Stainless Steel Plate](/products/steel-plate/stainless-steel-plate/304l-stainless-steel-plate)

304L stainless steel plate is the low-carbon form of 304, supplied as UNS S30403 for welded platework. Confirm thickness, width, length, finish and the purchasing standard.

![304 Stainless Steel Plate](/uploads/images/ss304-plate-7.webp)

### [304 Stainless Steel Plate](/products/steel-plate/stainless-steel-plate/304-stainless-steel-plate)

304 stainless steel plate (UNS S30400, ASTM A240) in mill and polished finishes for industrial fabrication, food processing equipment, and structural work. Provide thickness, width, length, and finish to receive a quotation.

![Duplex Steel Coil](/uploads/images/duplex-steel-coil-4.webp)

### [Duplex Steel Coil](/products/metal-steel-coil/stainless-steel-coils/duplex-steel-coil)

Duplex steel coil in 2205 (UNS S31803 / S32205, EN 1.4462) to ASTM A240, giving higher yield strength and chloride pitting resistance than 304/316 coil. Grades 2205, 2304 and 2507 are available; thickness, width, finish and coil build are confirmed at quotation.

```json
{"@context":"https://schema.org","@graph":[{"@type":"Organization","@id":"https://pipemanufactory.com/#organization","name":"Gangyou Steel Manufacture Company","alternateName":"Gangyou Steel","url":"https://pipemanufactory.com","logo":"https://pipemanufactory.com/uploads/images/ecfa6bb3-faec-48b0-8daa-81c94219bdaa.png","description":"Gangyou Steel supplies steel pipe, plate, coil, flanges, pipe fittings, fasteners, structural sections, round bar and industrial valves in carbon, stainless and alloy steel, from Foshan, China.","telephone":"+86-15875546993","email":"info@pipemanufactory.com","address":{"@type":"PostalAddress","streetAddress":"Gangtieshijie D7Qu 401 Jiagongqu er Road","addressLocality":"Foshan","addressRegion":"Guangdong","postalCode":"528000","addressCountry":"CN"},"contactPoint":{"@type":"ContactPoint","telephone":"+86-15875546993","email":"info@pipemanufactory.com","contactType":"customer service","availableLanguage":["en","es","de","fr","it","nl","pt","th","ko","vi","ja","id","ru","tr","zh-Hant","ar","no","hmn"]},"sameAs":["https://www.facebook.com/jerry.he.7731","https://www.instagram.com/jerry.he.7731"],"knowsAbout":["https://en.wikipedia.org/wiki/Steel","https://en.wikipedia.org/wiki/Stainless_steel","https://en.wikipedia.org/wiki/Carbon_steel","https://en.wikipedia.org/wiki/Alloy_steel","https://en.wikipedia.org/wiki/Duplex_stainless_steel","https://en.wikipedia.org/wiki/Pipe_(fluid_conveyance)","https://en.wikipedia.org/wiki/Piping_and_plumbing_fitting","https://en.wikipedia.org/wiki/Flange","https://en.wikipedia.org/wiki/Fastener","https://en.wikipedia.org/wiki/Valve","https://en.wikipedia.org/wiki/Structural_steel","https://en.wikipedia.org/wiki/Sheet_metal","https://en.wikipedia.org/wiki/Galvanization"],"hasCertification":[{"@type":"Certification","name":"PED 2014/68/EU Directive","issuedBy":{"@type":"Organization","name":"TUV Rheinland"},"validFrom":"2024-03-29"},{"@type":"Certification","name":"ASME U-Stamp Certification","issuedBy":{"@type":"Organization","name":"The American Society of Mechanical Engineers"},"validFrom":"2026-06-09"},{"@type":"Certification","name":"NORSOK M-650 Qualification","issuedBy":{"@type":"Organization","name":"DNV GL"},"validFrom":"2024-07-07"},{"@type":"Certification","name":"ISO 3834-2 Welding Certification","issuedBy":{"@type":"Organization","name":"TUV Nord"},"validFrom":"2024-08-11"},{"@type":"Certification","name":"Lloyd Register Type Approval","issuedBy":{"@type":"Organization","name":"Lloyd Register"},"validFrom":"2024-05-04"},{"@type":"Certification","name":"China CCC Certification","issuedBy":{"@type":"Organization","name":"CNCA"},"validFrom":"2024-08-31"},{"@type":"Certification","name":"ABS Steel Manufacturing Certificate","issuedBy":{"@type":"Organization","name":"American Bureau of Shipping"},"validFrom":"2024-04-17"},{"@type":"Certification","name":"FPC Certificate EN 1090-1","issuedBy":{"@type":"Organization","name":"TUV Rheinland"},"validFrom":"2024-06-24"}]},{"@type":"WebSite","@id":"https://pipemanufactory.com/#website","name":"Gangyou Steel Manufacture Company","url":"https://pipemanufactory.com","publisher":{"@id":"https://pipemanufactory.com/#organization"},"inLanguage":"en","potentialAction":{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https://pipemanufactory.com/products?q={search_term_string}"},"query-input":"required name=search_term_string"}}]}
{"@context":"https://schema.org","@graph":[{"@type":"WebPage","@id":"https://pipemanufactory.com/blog/steel-plate-complete-guide-types-grades-sta-103541230#webpage","url":"https://pipemanufactory.com/blog/steel-plate-complete-guide-types-grades-sta-103541230","name":"Steel Plate Grades: A36, A516, A572, 304 - Gangyou Steel","description":"Steel plate grades differ by duty. Compare A36, A516 Gr.70, A572 Gr.50, 304 and 2205 by yield strength, impact test temperature and thickness.","isPartOf":{"@id":"https://pipemanufactory.com/#website"},"inLanguage":"en","primaryImageOfPage":{"@type":"ImageObject","url":"https://pipemanufactory.com/uploads/images/blog_steel-plate-complete-guide-types-grades-sta-103541.webp"},"breadcrumb":{"@id":"https://pipemanufactory.com/blog/steel-plate-complete-guide-types-grades-sta-103541230#breadcrumb"},"mainEntity":{"@id":"https://pipemanufactory.com/blog/steel-plate-complete-guide-types-grades-sta-103541230#article"},"datePublished":"2026-06-16T04:00:00+08:00","dateModified":"2026-06-16T04:00:00+08:00"},{"@type":"BreadcrumbList","@id":"https://pipemanufactory.com/blog/steel-plate-complete-guide-types-grades-sta-103541230#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Home","item":"https://pipemanufactory.com/"},{"@type":"ListItem","position":2,"name":"Blog","item":"https://pipemanufactory.com/blog"},{"@type":"ListItem","position":3,"name":"Steel Plate Grades: A36, A516, A572, 304","item":"https://pipemanufactory.com/blog/steel-plate-complete-guide-types-grades-sta-103541230"}]},{"@type":"BlogPosting","@id":"https://pipemanufactory.com/blog/steel-plate-complete-guide-types-grades-sta-103541230#article","headline":"Steel Plate Grades: A36, A516, A572, 304","url":"https://pipemanufactory.com/blog/steel-plate-complete-guide-types-grades-sta-103541230","inLanguage":"en","isAccessibleForFree":true,"datePublished":"2026-06-16T04:00:00+08:00","dateModified":"2026-06-16T04:00:00+08:00","author":{"@type":"Person","name":"James Blue","jobTitle":"Piping Materials Specialist"},"publisher":{"@id":"https://pipemanufactory.com/#organization"},"mainEntityOfPage":{"@id":"https://pipemanufactory.com/blog/steel-plate-complete-guide-types-grades-sta-103541230#webpage"},"description":"Steel plate grades differ by duty. Compare A36, A516 Gr.70, A572 Gr.50, 304 and 2205 by yield strength, impact test temperature and thickness.","image":["https://pipemanufactory.com/uploads/images/blog_steel-plate-complete-guide-types-grades-sta-103541.webp"],"wordCount":822,"articleSection":"Blog","keywords":["construction","steel plate","cross","plate","pipe","cast","tee","iso"],"about":[{"@type":"Thing","name":"construction"},{"@type":"Thing","name":"steel plate"},{"@type":"Thing","name":"cross"},{"@type":"Thing","name":"plate"},{"@type":"Thing","name":"pipe"},{"@type":"Thing","name":"cast"},{"@type":"Thing","name":"tee"},{"@type":"Thing","name":"iso"}]}]}
{"@context":"https://schema.org","@type":"FAQPage","mainEntity":[{"@type":"Question","name":"When is ASTM A516 used instead of A36?","acceptedAnswer":{"@type":"Answer","text":"A516 is specified for pressure-containing parts such as vessels and boilers, while A36 is a general structural carbon steel grade without a pressure-vessel scope."}},{"@type":"Question","name":"What belongs on a steel plate enquiry?","acceptedAnswer":{"@type":"Answer","text":"Grade and standard with edition, thickness, width and length, heat treatment condition, impact test temperature, NDT scope, surface condition and quantity."}}]}
```