# ASTM vs EN vs JIS vs GB Pipe Standards

June 16, 2026 James Blue, Piping Materials Specialist

![ASTM vs EN vs JIS vs GB Pipe Standards](/uploads/images/blog_steel-pipe-standards-comparison-astm-vs-en-vs-1035.webp)

A grade that looks equivalent across ASTM, EN, JIS and GB is rarely interchangeable on paper alone. Substitution is an engineering decision that has to be evidenced by chemistry, mechanical properties, dimensions, impact testing and heat treatment condition, and then accepted against the code the project is built to. Use cross-reference tables to find candidates, not to approve them.

## What Each System Governs

ASTM standards are written by ASTM International and are widely referenced in North American, Middle Eastern and Southeast Asian projects. ASTM pipe specifications normally state chemistry limits, minimum mechanical properties, test requirements and permissible manufacturing routes, and grades are named by grade letter or number (Grade B, P11, TP316L).

EN standards are the European series. EN 10216 covers seamless pipe for pressure purposes - parts 1 to 5 by material family - and EN 10217 covers welded pipe for pressure purposes. Material names follow EN 10027, so a grade carries both a steel name such as P265GH and a material number such as 1.0425. For equipment installed in the European Union, the Pressure Equipment Directive 2014/68/EU applies and CE marking with the relevant conformity assessment is a separate requirement from the material standard itself.

JIS standards are the Japanese national series, with pipe specifications such as JIS G3454, G3456, G3458 and G3459 for pressure, high-temperature, alloy and stainless service. Grade prefixes encode the service, for example STPG, STS, STPA and SUS TP.

GB standards are the Chinese national series, where GB/T indicates a recommended standard. Common pipe specifications include GB/T 8163 for fluid service, GB/T 5310 for high-pressure boiler service, GB/T 9711 for line pipe and GB/T 14976 for stainless steel pipe for fluid transport. Grade designations may be numeric, such as 20#, or compositional, such as 12Cr1MoVG.

## Carbon Steel Pipe Cross-Reference

The pairings below are commonly used starting points for a substitution review, not approvals. Confirm the current edition of each specification before use.

| ASTM | EN | JIS | GB |
| --- | --- | --- | --- |
| A106 Gr.B | EN 10216-2 P265GH (1.0425) | JIS G3454 STPG410 | GB/T 8163 20# |
| A53 Gr.B | EN 10217-1 P235TR1 | JIS G3452 SGP | GB/T 3091 Q235B |
| API 5L Gr.B | EN 10208-2 L245MB | JIS G3457 STPG370 | GB/T 9711 L245 |
| API 5L X52 | EN 10208-2 L360NB | JIS G3456 STS480 | GB/T 9711 L360 |
| A333 Gr.6 | EN 10216-4 P355NL1 | JIS G3460 STPL380 | GB/T 18984 16MnDG |

## Alloy Steel Pipe Cross-Reference

| ASTM | EN | JIS | GB |
| --- | --- | --- | --- |
| A335 P11 | EN 10216-2 13CrMo4-5 (1.7335) | JIS G3458 STPA23 | GB/T 5310 15CrMoG |
| A335 P22 | EN 10216-2 10CrMo9-10 (1.7380) | JIS G3458 STPA24 | GB/T 5310 12Cr2MoG |
| A335 P91 | EN 10216-2 X10CrMoVNb9-1 (1.4903) | JIS G3458 STPA27 | GB/T 5310 10Cr9Mo1VNb |
| A335 P92 | EN 10216-2 X10CrWMoVNb9-2 (1.4901) | No direct equivalent | GB/T 5310 10Cr9W2MoVNb |

Cr-Mo grades are the clearest case for caution. Nominal chemistry can look close while heat treatment condition, tempering range and creep data differ, and a high-temperature design case is usually governed by allowable stress tables in the design code rather than by the material specification alone.

## Stainless Steel Pipe Cross-Reference

| ASTM | EN | JIS | GB |
| --- | --- | --- | --- |
| A312 TP304 | EN 10216-5 X5CrNi18-10 (1.4301) | JIS G3459 SUS304 TP | GB/T 14976 06Cr19Ni10 |
| A312 TP316 | EN 10216-5 X5CrNiMo17-12-2 (1.4401) | JIS G3459 SUS316 TP | GB/T 14976 06Cr17Ni12Mo2 |
| A312 TP304L | EN 10216-5 X2CrNi19-11 (1.4306) | JIS G3459 SUS304L TP | GB/T 14976 022Cr19Ni10 |
| A312 TP316L | EN 10216-5 X2CrNiMo17-12-2 (1.4404) | JIS G3459 SUS316L TP | GB/T 14976 022Cr17Ni12Mo2 |
| A312 TP321 | EN 10216-5 X6CrNiTi18-10 (1.4541) | JIS G3459 SUS321 TP | GB/T 14976 06Cr18Ni11Ti |

## What a Substitution Review Has to Check

Work through the same list every time, and record the result against each line:

- **Chemistry limits.** Carbon, manganese, sulphur and phosphorus limits differ between systems even for grades treated as equivalent. One documented example: ASTM A106 Grade B permits more carbon than EN 10216-2 P265GH, which matters for weldability and preheat.
- **Mechanical properties.** Compare minimum yield and tensile strength at the same thickness range and condition - for example ASTM A106 Grade B at 240 MPa minimum yield against EN 10216-2 P265GH at 265 MPa. Typical values are not minimum values.
- **Dimensions and tolerances.** Outside diameter series may not match, and wall thickness tolerance rules differ between specifications.
- **Impact testing.** Temperature, absorbed energy and specimen orientation are project decisions. A grade that is equivalent at ambient may have no qualified low-temperature data.
- **Heat treatment and delivery condition.** Normalised, quenched and tempered, or solution annealed change the properties you receive.
- **Supplementary requirements.** Many ASTM specifications add S1 to Sxx clauses for extra testing; ordering a bare grade number drops them by default.
- **Certification and code acceptance.** The design code, the inspector and - for the EU - the PED conformity route all have to accept the substitution.

A worked comparison of cross-system grade equivalence is set out in our article on [comparing steel grades across standards](/blog/metal-material-international-standard-equivale-103529130).

## Confirming the Standard on the Order

The purchase order should name the standard the engineering specification names, including edition or year, grade, and any supplementary requirements. If a substitute is being offered, the offer has to state which specification it is made to and provide the test results that support equivalence. Where the project is governed by a design code, the code acceptance is what decides the outcome.

## What to Confirm with Your Inquiry

Send these fields so a cross-standard enquiry can be answered with a defensible offer:

- Governing specification with edition, plus the design code the project is built to.
- Grade and - if substitution is allowed - the acceptable alternative standards.
- Product form and manufacturing route: for example [seamless carbon steel pipe](/products/steel-pipe/carbon-steel-pipe/seamless-carbon-steel-pipe), [API 5L Grade B seamless line pipe](/products/steel-pipe/carbon-steel-pipe/api-5l-grade-b-seamless-pipe), [ASTM A335 P11 Cr-Mo pipe](/products/steel-pipe/alloy-steel-pipe/astm-a335-p11-seamless-cr-mo-alloy-steel-pipe) or [ASTM A312 TP316L stainless pipe](/products/steel-pipe/stainless-steel-pipe/316l-stainless-steel-pipe).
- Size range, schedule or wall thickness, and length.
- Heat treatment condition and delivery condition.
- Impact test temperature and absorbed energy required, if any.
- Inspection scope and certificate type, including third-party inspection where required.
- Quantity and delivery term.

## Frequently Asked Questions

### Can ASTM, EN, JIS and GB grades replace each other automatically?

No. A substitution needs comparison of chemistry, mechanical properties, dimensions, impact testing and heat treatment against the governing code.

### Which standard should appear on the purchase order?

The standard named by the engineering specification, including edition, grade and any supplementary requirements, plus the design code the project is built to.

Share [Facebook](https://www.facebook.com/sharer/sharer.php?u=https%3A%2F%2Fpipemanufactory.com%2Fblog%2Fsteel-pipe-standards-comparison-astm-vs-en-vs-103541751) [X](https://twitter.com/intent/tweet?url=https%3A%2F%2Fpipemanufactory.com%2Fblog%2Fsteel-pipe-standards-comparison-astm-vs-en-vs-103541751) [LinkedIn](https://www.linkedin.com/shareArticle?url=https%3A%2F%2Fpipemanufactory.com%2Fblog%2Fsteel-pipe-standards-comparison-astm-vs-en-vs-103541751)

[Send Inquiry](/inquiry?ref=steel-pipe-standards-comparison-astm-vs-en-vs-103541751)

Latest Posts

- [!\[Steel Pipe Lead Time from China Explained\](/uploads/images/blog_steel-pipe-lead-time-from-china-complete-guid-1035.webp) Steel Pipe Lead Time from China Explained](/blog/steel-pipe-lead-time-from-china-complete-guid-103565829)
- [!\[Steel Pipe Export Packaging and Shipping\](/uploads/images/blog_steel-pipe-export-packaging-and-shipping-guide-103.webp) Steel Pipe Export Packaging and Shipping](/blog/steel-pipe-export-packaging-and-shipping-guide-103565688)
- [!\[How to Audit a Chinese Steel Pipe Factory\](/uploads/images/blog_how-to-audit-a-chinese-steel-pipe-factory-com-1035.webp) How to Audit a Chinese Steel Pipe Factory](/blog/how-to-audit-a-chinese-steel-pipe-factory-com-103565697)

## Related Products

[View More](/products)

![2507 Super Duplex Stainless Steel Plate (UNS S32750)](/uploads/images/duplex-steel-plate-sheet-3.webp)

### [2507 Super Duplex Stainless Steel Plate (UNS S32750)](/products/steel-plate/stainless-steel-plate/2507-super-duplex-stainless-steel-plate-uns-s32750)

2507 super duplex stainless steel plate for projects that specify S32750 (2507). S32760 is a related grade with slight elemental differences and must be specified separately. Confirm the requested grade, applicable product standard and dimensions before quotation.

![304L Stainless Steel Plate](/uploads/images/ss304-plate-9.webp)

### [304L Stainless Steel Plate](/products/steel-plate/stainless-steel-plate/304l-stainless-steel-plate)

304L stainless steel plate is the low-carbon form of 304, supplied as UNS S30403 for welded platework. Confirm thickness, width, length, finish and the purchasing standard.

![304 Stainless Steel Plate](/uploads/images/ss304-plate-7.webp)

### [304 Stainless Steel Plate](/products/steel-plate/stainless-steel-plate/304-stainless-steel-plate)

304 stainless steel plate (UNS S30400, ASTM A240) in mill and polished finishes for industrial fabrication, food processing equipment, and structural work. Provide thickness, width, length, and finish to receive a quotation.

![Duplex Steel Coil](/uploads/images/duplex-steel-coil-4.webp)

### [Duplex Steel Coil](/products/metal-steel-coil/stainless-steel-coils/duplex-steel-coil)

Duplex steel coil in 2205 (UNS S31803 / S32205, EN 1.4462) to ASTM A240, giving higher yield strength and chloride pitting resistance than 304/316 coil. Grades 2205, 2304 and 2507 are available; thickness, width, finish and coil build are confirmed at quotation.

```json
{"@context":"https://schema.org","@graph":[{"@type":"Organization","@id":"https://pipemanufactory.com/#organization","name":"Gangyou Steel Manufacture Company","alternateName":"Gangyou Steel","url":"https://pipemanufactory.com","logo":"https://pipemanufactory.com/uploads/images/ecfa6bb3-faec-48b0-8daa-81c94219bdaa.png","description":"Gangyou Steel supplies steel pipe, plate, coil, flanges, pipe fittings, fasteners, structural sections, round bar and industrial valves in carbon, stainless and alloy steel, from Foshan, China.","telephone":"+86-15875546993","email":"info@pipemanufactory.com","address":{"@type":"PostalAddress","streetAddress":"Gangtieshijie D7Qu 401 Jiagongqu er Road","addressLocality":"Foshan","addressRegion":"Guangdong","postalCode":"528000","addressCountry":"CN"},"contactPoint":{"@type":"ContactPoint","telephone":"+86-15875546993","email":"info@pipemanufactory.com","contactType":"customer service","availableLanguage":["en","es","de","fr","it","nl","pt","th","ko","vi","ja","id","ru","tr","zh-Hant","ar","no","hmn"]},"sameAs":["https://www.facebook.com/jerry.he.7731","https://www.instagram.com/jerry.he.7731"],"knowsAbout":["https://en.wikipedia.org/wiki/Steel","https://en.wikipedia.org/wiki/Stainless_steel","https://en.wikipedia.org/wiki/Carbon_steel","https://en.wikipedia.org/wiki/Alloy_steel","https://en.wikipedia.org/wiki/Duplex_stainless_steel","https://en.wikipedia.org/wiki/Pipe_(fluid_conveyance)","https://en.wikipedia.org/wiki/Piping_and_plumbing_fitting","https://en.wikipedia.org/wiki/Flange","https://en.wikipedia.org/wiki/Fastener","https://en.wikipedia.org/wiki/Valve","https://en.wikipedia.org/wiki/Structural_steel","https://en.wikipedia.org/wiki/Sheet_metal","https://en.wikipedia.org/wiki/Galvanization"],"hasCertification":[{"@type":"Certification","name":"PED 2014/68/EU Directive","issuedBy":{"@type":"Organization","name":"TUV Rheinland"},"validFrom":"2024-03-29"},{"@type":"Certification","name":"ASME U-Stamp Certification","issuedBy":{"@type":"Organization","name":"The American Society of Mechanical Engineers"},"validFrom":"2026-06-09"},{"@type":"Certification","name":"NORSOK M-650 Qualification","issuedBy":{"@type":"Organization","name":"DNV GL"},"validFrom":"2024-07-07"},{"@type":"Certification","name":"ISO 3834-2 Welding Certification","issuedBy":{"@type":"Organization","name":"TUV Nord"},"validFrom":"2024-08-11"},{"@type":"Certification","name":"Lloyd Register Type Approval","issuedBy":{"@type":"Organization","name":"Lloyd Register"},"validFrom":"2024-05-04"},{"@type":"Certification","name":"China CCC Certification","issuedBy":{"@type":"Organization","name":"CNCA"},"validFrom":"2024-08-31"},{"@type":"Certification","name":"ABS Steel Manufacturing Certificate","issuedBy":{"@type":"Organization","name":"American Bureau of Shipping"},"validFrom":"2024-04-17"},{"@type":"Certification","name":"FPC Certificate EN 1090-1","issuedBy":{"@type":"Organization","name":"TUV Rheinland"},"validFrom":"2024-06-24"}]},{"@type":"WebSite","@id":"https://pipemanufactory.com/#website","name":"Gangyou Steel Manufacture Company","url":"https://pipemanufactory.com","publisher":{"@id":"https://pipemanufactory.com/#organization"},"inLanguage":"en","potentialAction":{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https://pipemanufactory.com/products?q={search_term_string}"},"query-input":"required name=search_term_string"}}]}
{"@context":"https://schema.org","@graph":[{"@type":"WebPage","@id":"https://pipemanufactory.com/blog/steel-pipe-standards-comparison-astm-vs-en-vs-103541751#webpage","url":"https://pipemanufactory.com/blog/steel-pipe-standards-comparison-astm-vs-en-vs-103541751","name":"ASTM vs EN vs JIS vs GB Pipe Standards - Gangyou Steel","description":"Cross-standard pipe substitution needs more than a matching grade name. Compare chemistry, mechanical properties, dimensions and impact testing first.","isPartOf":{"@id":"https://pipemanufactory.com/#website"},"inLanguage":"en","primaryImageOfPage":{"@type":"ImageObject","url":"https://pipemanufactory.com/uploads/images/blog_steel-pipe-standards-comparison-astm-vs-en-vs-1035.webp"},"breadcrumb":{"@id":"https://pipemanufactory.com/blog/steel-pipe-standards-comparison-astm-vs-en-vs-103541751#breadcrumb"},"mainEntity":{"@id":"https://pipemanufactory.com/blog/steel-pipe-standards-comparison-astm-vs-en-vs-103541751#article"},"datePublished":"2026-06-16T04:00:00+08:00","dateModified":"2026-06-16T04:00:00+08:00"},{"@type":"BreadcrumbList","@id":"https://pipemanufactory.com/blog/steel-pipe-standards-comparison-astm-vs-en-vs-103541751#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Home","item":"https://pipemanufactory.com/"},{"@type":"ListItem","position":2,"name":"Blog","item":"https://pipemanufactory.com/blog"},{"@type":"ListItem","position":3,"name":"ASTM vs EN vs JIS vs GB Pipe Standards","item":"https://pipemanufactory.com/blog/steel-pipe-standards-comparison-astm-vs-en-vs-103541751"}]},{"@type":"BlogPosting","@id":"https://pipemanufactory.com/blog/steel-pipe-standards-comparison-astm-vs-en-vs-103541751#article","headline":"ASTM vs EN vs JIS vs GB Pipe Standards","url":"https://pipemanufactory.com/blog/steel-pipe-standards-comparison-astm-vs-en-vs-103541751","inLanguage":"en","isAccessibleForFree":true,"datePublished":"2026-06-16T04:00:00+08:00","dateModified":"2026-06-16T04:00:00+08:00","author":{"@type":"Person","name":"James Blue","jobTitle":"Piping Materials Specialist"},"publisher":{"@id":"https://pipemanufactory.com/#organization"},"mainEntityOfPage":{"@id":"https://pipemanufactory.com/blog/steel-pipe-standards-comparison-astm-vs-en-vs-103541751#webpage"},"description":"Cross-standard pipe substitution needs more than a matching grade name. Compare chemistry, mechanical properties, dimensions and impact testing first.","image":["https://pipemanufactory.com/uploads/images/blog_steel-pipe-standards-comparison-astm-vs-en-vs-1035.webp"],"wordCount":960,"articleSection":"Blog","keywords":["stainless steel pipe","carbon steel pipe","alloy steel pipe","stainless steel","carbon steel","alloy steel","steel pipe","chemical"],"about":[{"@type":"Thing","name":"stainless steel pipe"},{"@type":"Thing","name":"carbon steel pipe"},{"@type":"Thing","name":"alloy steel pipe"},{"@type":"Thing","name":"stainless steel"},{"@type":"Thing","name":"carbon steel"},{"@type":"Thing","name":"alloy steel"},{"@type":"Thing","name":"steel pipe"},{"@type":"Thing","name":"chemical"}]}]}
{"@context":"https://schema.org","@type":"FAQPage","mainEntity":[{"@type":"Question","name":"Can ASTM, EN, JIS and GB grades replace each other automatically?","acceptedAnswer":{"@type":"Answer","text":"No. A substitution needs comparison of chemistry, mechanical properties, dimensions, impact testing and heat treatment against the governing code."}},{"@type":"Question","name":"Which standard should appear on the purchase order?","acceptedAnswer":{"@type":"Answer","text":"The standard named by the engineering specification, including edition, grade and any supplementary requirements, plus the design code the project is built to."}}]}
```